MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Delrin® 150XV BK602 Acetal Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Delrin® 150XV BK602 is a high viscosity acetal homopolymer for extrusion. It has excellent thermal stability, low die deposit, and can be processed in void-free thick section rods and plates.

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Melt Flow 2.4 g/10 min
@Load 2.16 kg,
Temperature 109 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 73.0 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 30 %
@Temperature 23.0 °C
ISO 527
Elongation at Yield 15 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 3200 MPa
@Temperature 23.0 °C
ISO 527
Flexural Modulus 3000 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 195 - 205 °CExtrusion
 200 °CExtrusion
 215 °CInjection Molding
 210 - 220 °CInjection Molding
Mold Temperature 90.0 °CInjection Molding
 80.0 - 100 °CInjection Molding
Drying Temperature 80.0 °CExtrusion
 80.0 °CInjection Molding
Dry Time 2 - 4 hourExtrusion
 2 - 4 hourInjection Molding
Moisture Content <= 0.20 %Extrusion
 <= 0.20 %Injection Molding
 
Descriptive Properties
AppearanceBlack
GenericAcetal (POM) Homopolymer
Part Marking Code, ISO 11469>POM<
Polymer FamilyPOM
Polymer TypePOM Homopolymer
Processing MethodExtrusion
Product CategoryExtrusion Resins
 Unreinforced Resins
Region Available - AmericasYes
Region Available - Asia/PacificYes
Region Available - EuropeYes
Resin IdentificationPOM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTA5072 / 126085

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.