MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Diofan® A610 Polyvinylidene Chloride (PVDC)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: DIOFAN® A610 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features exceptional barrier properties to water vapor and oxygen. DIOFAN® A610 is a high surface tension latex; the addition of a convenient surfactant will enable to obtain a good quality coating as well as the addition of a coalescent agent to facilitate film formation at low temperature (< 10°C). DIOFAN® A610, as chlorinated based latex, combines also fire retardant properties. END USES: - Barrier and sealing coatings - Flame resistant coatings - Fibers and textile coatings Where substrates can be concrete, cement, wood, gypsum, paper, fiberboard, ...

Additional Information: DELIVERY AND STORAGE: - DIOFAN® A610 will be delivered in bulk or in Intermediate Bulk Containers (IBC). Storage of bulk latex is in reservoirs made of stainless steel, HDPE, rigid PVC or glass fiber reinforced polyester. In particular, metals like iron, zinc, aluminum and copper as well as alloys like brass and bronze have to be avoided for contact with the dispersions. To prevent from drying by evaporation, keep the vessel tightly closed. To avoid degradation, store the product preferably between 10 and 25°C. REGULATORY INFORMATION - The monomers used for the production of DIOFAN® A610 comply with the requirements of the EU Commission Regulation No. 10/2011 of 14 January 2011. - DIOFAN® A610 complies fully with the U.S. Federal Food, Drug and Cosmetic Act and all applicable food additive regulations. - The monomers used for the production of DIOFAN® A610 comply with the Regulation (EC) 1907/2006 of the European Parliament and of the Council of 18 December 2006 concerning the Registration, Evaluation, Authorization and Restriction of Chemicals (REACH). - SolVin will provide further certification documentation upon request ISO CERTIFICATION: - The implemented management system for the production, internal transfer and delivery, design and development of DIOFAN vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/cc
 1.65 g/ccFilm
Solids Content 60 %
pH 1.5
Water Vapor Transmission 14.0 g/m²/day
@Temperature 38.0 °C
90% RH; 1 µm
Oxygen Transmission Rate >= 40.0 cc/m²/day25°C, 1.0 µm, 85% RH
Surface Tension 54 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 16.0 °CFilm; DSC
 
Descriptive Properties
Agency RatingsEC 1907/2006 (REACH)
 EU No 10/2011
AppearanceMilky white liquid
 White
AvailabilityAsia Pacific
 Europe
 North America
Emulsion TypeAnionic
FeaturesBarrier Resin
 Flame Retardant
 Non-Toxic
Filmability11°CMinimum Film Forming Temperature
FormsLiquid
GenericPVDC
UsesCoating Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Diofan® A602 Polyvinylidene Chloride (PVDC)
Syensqo (Solvay Specialty Polymers) Diofan® P530 Polyvinylidene Chloride (PVDC)
Syensqo (Solvay Specialty Polymers) Diofan® A 036 Polyvinylidene Chloride (PVDC)
Syensqo (Solvay Specialty Polymers) Diofan® P510 Polyvinylidene Chloride (PVDC)
Syensqo (Solvay Specialty Polymers) Ixan® PVS 706 Polyvinylidene Chloride (PVDC)

PSOL8Y7638 / 135701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.