MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite side. Mylar® RB52 is essentially RL52 with a barrier layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Mylar® RB52 is available in nominal 50 gauge. Mylar® RB52 is designed to seal to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), and polystyrene (HIPS). However, Mylar® RB52 produces weak seals to polypropylene at lower seal temperatures (below 350°F) - especially under chilled conditions, and therefore is not recommended. (RL "40 Series" is recommended for these applications. Mylar® RB52 has the same type heat seal layer as Mylar® RL51, but the thickness of the heat seal layer and the heat seal strengths of Mylar® RB52 are intermediate between Mylar® RL51 and Mylar® RL53. RB52 produces more ductile seals under refrigerated or frozen conditions and seals better to polystyrene containers than either RL32 or RL42. Like RL51, Mylar® RB52 has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures). Mylar® RB52 can withstand freezing temperatures down to -40°F, and foods can be heated or cooked in contact with this film if food temperatures do not exceed 250°F. The oriented polyester base film will begin to distort in the range of 425-450°F.

Special Features: Corona Treatment: Mylar® RB52 is not available with corona treatment on the opposite side of film from the heat seal layer. However, the PVdC surface already on that side of the film is suitable for printing and laminating.

Approvals: FDA Food Contact Status - Mylar® RB52 polyester film complies with the U.S. Food and Drug Administration Regulation 21 CFR 177.1630 for use in contact with all types of food, excluding alcoholic beverages, at food temperatures not to exceed 250°F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccTypical Mylar®; ASTM D1505
Water Vapor Transmission 0.500 g/100 in²/day
@Temperature 38.0 °C
90% RH; ASTM F1249
Thickness 0.500 mil
Coating Weight 16.2 lb/ream0.5 m2; ASTM E252
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882A
Film Elongation at Break, TD 80 %ASTM D882A
Tensile Modulus 550000 psiASTM D882
Graves Tear Strength 0.700 pliASTM D1004
Film Tensile Strength at Break, MD 25000 psiASTM D882A
Film Tensile Strength at Break, TD 35000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)0.5 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)26000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® RSX Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge

PDTZ9398 / 139718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.