MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ FA-210 Engineered Specialty Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: JFoam™ FA-210-R is the resin component of a two part polyurethane system, which when with the T component, Isocyanate, will produce an HFC-245fa and water co-blown rigid polyurethane foam system. FA-210 can be used in a variety of specialized low density molding and void filling applications. This foam product in its finished form is flame retardant and can meet some Military Specification requirements.

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccR Component, Polyol Blend
 1.24 g/ccT Component, Polymeric MDI
 2.10 lb/ft³Cup density, #10
 2.11 lb/ft³Core; ASTM D1622
 2.41 lb/ft³Molded, overall; ASTM D1622
Water Absorption 2.93 %by volume; ASTM D-2842
 72 %weight (per MIL-PRF-26514G); ASTM D-2842
Viscosity 200 cPT Component, Polymeric MDI
 1080 cPR Component, Polyol Blend
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 24.12 psiPerpendicular; ASTM D1623
 34.0 psiParallel; ASTM D1623
Tensile Modulus 809.02 psiPerpendicular; ASTM D1623
 2269.89 psiParallel; ASTM D1623
Compressive Strength 26.56 psiPerpendicular, 10% deflection; ASTM D1621
 45.41 psiParallel, 10% deflection; ASTM D1621
Compressive Modulus 430.4 psiPerpendicular; ASTM D1621
 963.97 psiParallel; ASTM D1621
Shear Modulus 910.36 ksiParallel; ASTM C273
 1161.27 ksiPerpendicular; ASTM C273
Shear Strength 18.49 psiParallel; ASTM C273
 21.76 psiPerpendicular; ASTM C273
Compression Set 0.98 %MIL-P-21929C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.04
@Frequency 1e+6 Hz
ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.174 BTU-in/hr-ft²-°FASTM C518
 
Processing PropertiesOriginal ValueComments
Gel Time 1.083 min
Shelf Life 6.00 Month
 
Descriptive Properties
Closed Cell Content88.2%ASTM D6226
Dimensional Stability+13% ChangeCold Aging at -20°F (-29°C), 14 days, ASTM D2126
 +8% ChangeHeat Aging at 158°F (70°C), 14 days, ASTM D2126
Hand Mix Reactivity24 secCream Time
Mixing Ratio0.38R Component, Polyol Blend
 0.62T Component, Polymeric MDI

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lendell Supersoft Foams
Mearthane Durethane™ C Foams DCF and DCM Polyurethane
Lendell Medisponge®
Lendell Nolatex® Latex Free Foam
CIMBAR Miti-Wite B1 Chemically Purified White Barite (BaSO4)

PJSIX021 / 190948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.