MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness and ingot homogeneity, and to enhance mechanical properties.

Mechanical Properties from FMS-1111 Specification

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 190 ksi
Tensile Strength, Yield 1241 MPa
Elongation at Break 15 %
Reduction of Area 65 %
Modulus of Elasticity 27600 ksi
Charpy Impact 81.0 J
@Temperature -17.8 °C
V-notch
 
Processing PropertiesOriginal ValueComments
Processing Temperature 166 °CCritical Temperaure Mf
 327 °CCritical Temperaure Ms
 624 °CCritical Temperaure Ac1
 793 °CCritical Temperaure Ac3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.13 %
Chromium, Cr 2.0 %
Cobalt, Co 8.0 %
Iron, Fe 78.72 %
Manganese, Mn 0.10 %
Molybdenum, Mo 1.0 %
Nickel, Ni 10 %
Silicon, Si 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel
HY-100 Steel
HY-130 Steel

NTIMK020 / 19368

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.