MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Acheson™ SS 24600 Conductive Resin
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: SS 24600 is one of a series of Acheson coatings designed to provide controlled electrical properties. SS 24600 is a dispersion of finely divided graphite in a thermoplastic resin that rapidly air dries to form a flexible conductive coating. It is designed to be applied by typical spray, flexographic or gravure print techniques.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Viscosity 3500 cP
Thickness 5.00 - 12.0 microns
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.10 - 40 ohm
 
Processing PropertiesOriginal ValueComments
Cure Time 600 sec
 
Descriptive Properties
Binder SystemPVC resin
Conductive Filler TypeGraphite
Material TypeDispersion
Solvent Systemn-propyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI LATISTAT 87/28-09 G/10 Polycarbonate, 10% Glass Fiber Reinforced Conductive Plastic
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene
Lanxess Mersolat® H68 Plastic Additive, Emulsifier
Henkel Hysol EA 9150 Composite Resin
Henkel Electrodag® PD-056 Conductive Resin

PFLEXCM53 / 179455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.