MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinoid 2002-4A Phenolic Molding, Fabric Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Data provided by the manufacturer.

Resinoid 2002-4A is a fabric reinforced, two-step phenolic molding compound. It has been modified to meet gear requirements and other stressed applications. It possesses excellent impact and flexural strength. It is available in bulk form and is recommended for compression or transfer molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792A
Water Absorption 0.60 %24 hours R.T.; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmPositive Mold; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 55.0 MPaASTM D651
Flexural Strength 97.0 MPaASTM D790
Flexural Modulus 11.0 GPaASTM D790
Compressive Strength 150 MPaASTM D695
Izod Impact, Notched 2.10 ft-lb/inASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.8 kV/mmShort Time; Dry; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 177 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 150 - 175 °CASTM D957
Injection Pressure 14.0 - 28.0 MPaMolding Pressure –Compression
 
Descriptive Properties
Bulk Factor10-12ASTM D1895
ColorBlack
FormChopped Fabric

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPHR0IA / 253984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.