Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |