MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Bearing Material

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Water Absorption 0.090 %ASTM D570
Deformation 0.030 %ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 91ASTM D785
Tensile Strength 57.0 MPa
@Temperature 260 °C
D-1780 Specimen
 116 MPa
@Temperature 22.8 °C
ASTM D638
Elongation at Break 3.0 %
@Temperature 22.8 °C
ASTM D638
 9.7 %
@Temperature 260 °C
D-1780 Specimen
Modulus of Elasticity 2.612 GPa
@Temperature 260 °C
D 1780 Specimen
 6.003 GPa
@Temperature 22.8 °C
ASTM D638
Flexural Strength 99.0 MPa
@Temperature 260 °C
ASTM D790
 195 MPa
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 3560 MPa
@Temperature 260 °C
ASTM D790
 6231 MPa
@Temperature 22.8 °C
ASTM D790
Compressive Strength 414 MPa
@Temperature 260 °C
ASTM D695
 481 MPa
@Temperature 22.8 °C
ASTM D695
 96.0 MPa
@Strain 10 %,
Temperature 260 °C
ASTM D695
 222 MPa
@Strain 10 %,
Temperature 22.8 °C
ASTM D695
Compressive Modulus 1663 MPa
@Temperature 260 °C
ASTM D695
 2594 MPa
@Temperature 22.8 °C
ASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 44.0 µm/m-°C
@Temperature 23.0 - 300 °C
ASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber

PDU1999m / 183711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.