MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
KaMin Polyfil® WC Kaolin Clay - Calcined
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Polyfil®WC clay is an organo-functional calcined kaolin clay used in Wire and Cable and other thermoplastic applications. It is designed to reduce water vapor transmission, yields excellent wet and dry electrical properties, and also long-term stability in EPR and cross-linked polyethylene. Calcined clays have low conductivity due to the elimination of bound water during the calcined process. Compounds with calcined clays extrude smoothly and reduce stickiness in processing.

Industry: Rubber & Plastic

Uses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & Cable

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Brightness 91 %Reflectance (TAPPI)
Oil Absorption 54 %
Moisture Absorption at Equilibrium <= 0.5 %As Produced
Particle Size 1.4 µmAverage Stokes Equivalent Diameter
 3.2 µmMedian (Malvern Laser)
Particle Mesh Size 325 Mesh0.01% Retained
pH 6100 g/250 ml H2O Slurry
Specific Surface Area 7.0 - 9.0 m²/gBET
 
Descriptive Properties
CAS NumberProprietary
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
CoorsTek Tungsten Carbide, WC
KaMin Polyfil® 90 Kaolin Clay - Calcined
KaMin Polyfil® 80 Kaolin Clay - Calcined
KaMin Polyfil® 70 Kaolin Clay - Calcined

CKAMAN945 / 178416

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.