MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 - 0.980 g/ccAverage value: 0.944 g/cc Grade Count:101
Viscosity 140 - 40000 cP
@Temperature 121 - 190 °C
Average value: 495000 cP Grade Count:42
 300000 - 1.90e+6 cP
@Temperature 190 - 190 °C
Average value: 495000 cP Grade Count:22
 300000 - 1.90e+6 cP
@Shear Rate 50.0 - 50.0 1/s
Average value: 495000 cP Grade Count:22
Environmental Stress Crack Resistance >= 300 hour
@Temperature 50.0 - 50.0 °C
Average value: 300 hour Grade Count:3
 >= 300 hour
@Thickness 2.00 - 2.00 mm
Average value: 300 hour Grade Count:3
Vinyl Acetate Content 17.0 - 44.0 %Average value: 26.8 % Grade Count:50
Melt Flow 0.550 - 900 g/10 minAverage value: 123 g/10 min Grade Count:98
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40.0 - 90.0Average value: 72.6 Grade Count:52
Hardness, Shore D 14.0 - 39.0Average value: 23.5 Grade Count:35
Tensile Strength, Ultimate 1.50 - 27.0 MPaAverage value: 6.34 MPa Grade Count:59
Tensile Strength, Yield 2.70 - 6.50 MPaAverage value: 4.82 MPa Grade Count:4
Film Elongation at Break, MD 300 - 800 %Average value: 491 % Grade Count:10
Film Elongation at Break, TD 460 - 950 %Average value: 747 % Grade Count:9
Elongation at Break 50.0 - 1300 %Average value: 626 % Grade Count:56
Modulus of Elasticity 0.00300 - 0.100 GPaAverage value: 0.0677 GPa Grade Count:3
Flexural Modulus 0.00440 - 0.0427 GPaAverage value: 0.0225 GPa Grade Count:34
Secant Modulus, MD 0.0469 - 0.145 GPaAverage value: 0.0846 GPa Grade Count:8
Secant Modulus, TD 0.0503 - 0.179 GPaAverage value: 0.0984 GPa Grade Count:8
Dart Drop, Total Energy 24.4048 - 24.4048 J
@Temperature -40.0 - -40.0 °C
Average value: 24.4 J Grade Count:1
Dart Drop 4.92 - 23.6 g/micronAverage value: 10.8 g/micron Grade Count:7
Seal Strength 1200 - 4500 g/25 mmAverage value: 2860 g/25 mm Grade Count:4
Film Tensile Strength at Break, MD 7.58 - 31.7 MPaAverage value: 24.4 MPa Grade Count:10
Film Tensile Strength at Break, TD 15.9 - 31.0 MPaAverage value: 23.7 MPa Grade Count:9
 
Thermal PropertiesOriginal ValueComments
Melting Point 48.0 - 112 °CAverage value: 75.6 °C Grade Count:100
Maximum Service Temperature, Air 51.7 - 78.9 °CAverage value: 68.2 °C Grade Count:29
Vicat Softening Point 37.8 - 95.0 °CAverage value: 54.9 °C Grade Count:77
Minimum Service Temperature, Air -45.6 - -17.8 °CAverage value: -28.9 °C Grade Count:29
Ring & Ball Softening Point 76.0 - 183 °CAverage value: 110 °C Grade Count:27
 
Optical PropertiesOriginal ValueComments
Haze 0.800 - 4.50 %Average value: 2.89 % Grade Count:8
Gloss 72.0 - 90.0 %Average value: 79.5 % Grade Count:8
Transmission, Visible 80.0 - 90.0 %Average value: 83.3 % Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 315 °CAverage value: 235 °C Grade Count:42
Nozzle Temperature 185 - 275 °CAverage value: 234 °C Grade Count:22
Adapter Temperature 185 - 285 °CAverage value: 224 °C Grade Count:4
Die Temperature 185 - 285 °CAverage value: 224 °C Grade Count:4
Melt Temperature 150 - 305 °CAverage value: 207 °C Grade Count:17
Pot Life 0.0833 - 1.00 minAverage value: 0.449 min Grade Count:29

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate

O4108 / 78295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.