MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Elexar® EL 8732R Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-8732R is high performance, flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar® EL-8730A is a high durometer grade, RoHS compliant grade. This grade is UL listed and is suitable for both injection molding and extrusion.

Features: Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated; Heat Aging Resistant; High Elasticity; High Elongation; High Specific Gravity; High Tensile Strength; Medium Flow; Ozone Resistant; Sunlight Resistant (720 hours); UV Resistant; Weather Resistant

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81ASTM D2240
Tensile Strength at Break 12.4 MPa
@Thickness 0.508 mm
Extruded Tape, Die C, 20 in/min; ASTM D412
 11.16 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 11.904 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
Tensile Stress at Strain 470 psi
@Strain 100 %,
Thickness 0.508 mm
Extruded Tape, Die C, 20 in/min; ASTM D412
 690 psi
@Strain 300 %,
Thickness 0.508 mm
Extruded Tape, Die C, 20 in/min; ASTM D412
Elongation at Break 650 %
@Thickness 0.508 mm
Extruded Tape, Die C, 20 in/min; ASTM D412
 604.5 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 663 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.50e+14 ohm-cm
@Temperature 50.0 °C
ASTM D257
 1.40e+16 ohm-cm
@Temperature 22.8 °C
ASTM D257
Dielectric Constant 2.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 640 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FContinuous; UL 1581
Brittleness Temperature -76.0 °FASTM D746
Flammability, UL94 V-20.12 in, All Colors
Oxygen Index 23 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 420 °F
Middle Barrel Temperature 415 - 430 °F
Front Barrel Temperature 430 - 440 °F
Nozzle Temperature 430 - 445 °F
Zone 1 380 - 410 °F
Zone 2 390 - 420 °F
Zone 3 415 - 430 °F
Zone 4 430 - 445 °F
Zone 5 430 - 440 °F
Die Temperature 430 - 445 °F
Melt Temperature 430 - 445 °FProcessing Temp
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer

PTEKNO782 / 128963

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.