Description: Liquid two-part epoxy resin adhesive. Its low viscosity makes it suitable for bonding by injection process and repairing by war lay up of fabrics. Features: - Room temperature cure (= 18oC/64oF)
- Outstanding mechanical properties over a wide range of temperature (-55oC/-67oF to 180oC/356oF)
- Low viscosity
Information provided by Hexcel Corporation. |