MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Geniosil® XL 10 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C5H12O3Si

CAS No.: 2768-02-7

Properties: Pipes and cables produced from silane-crosslinked polyethylene (PE-Xb) using GENIOSIL® XL 10 are more resistant to heat and weathering than products made from non-crosslinked polyethylene. They also have improved electrical properties. The storage stability is greatly enhanced in formulations of silane crosslinking adhesives and sealants. Use of GENIOSIL® XL 10 as a co-monomer in polymer dispersions results in binders which exhibit much improved wet scrub resistance and higher abrasion resistance thanks to crosslinking and improved adhesion to the substrate.

Special features: GENIOSIL® XL 10 is an alkoxyvinylsilane.It´s a clear, colorless liquid with a characteristic odor.The silane hydrolyzes in the presence of moisture (methanol is released) to form silanols, which can then react with themselves to produce siloxanes.

Application: GENIOSIL® XL 10 is used in the production of pipes and cables made of silane-crosslinked polyethylene (PE-Xb), as a water scavenger during the production of silane-crosslinking adhesive and sealant formulations, and as co-monomers in the production of silane modified binders for surface coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccDIN 51757
Viscosity 0.60 cPdynamic; DIN 51562
Molecular Weight 148.2 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 122 °C
@Pressure 0.1013 MPa
Flash Point 25.0 °CISO 13736
Ignition Temperature 240 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.391
 
Descriptive Properties
Content<0.3%Dimer
 <0.3%Methanol
 <10 mg/kgHydrolyzable chloride (as HCl)
Purity>99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Geniosil® GF 58 US Silane
Dow Z-6030 SILANE
Wacker Geniosil® GF 93 Silane
Wacker Geniosil® GF 80 US Silane

PWACK9332 / 204861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.