MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical LUTENE® XL8080UCS XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: Cross-linkable polyethylene compound for high and extra high voltage power cable insulation with rated voltage up to 230kV

LUTENE® XL8080UCS is a superior cleanliness version for high and extra high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination.

Specification: LUTENE® XL8080UCS meets the property requirement of the following material specifications.
? AEIC CS9
? AEIC CS8
? KSC 3611
? ICEA S-94-649
? IEC 60502
? IEC 60840
? IEC 62067

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³Base Resin; ASTM D1505
Deformation <= 15 %
@Pressure 0.200 MPa,
Temperature 200 °C
<= 15 %
@Pressure 29.0 psi,
Temperature 392 °F
Permanent, Hot Set Test; IEC 60811-2-1
Degree of Crosslinking >= 80 %>= 80 %ASTM D2765A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 19.7 MPa>= 2860 psi200 mm/min; ASTM D638
 >= 17.7 MPa
@Treatment Temp. 135 °C,
Time 605000 sec
>= 2570 psi
@Treatment Temp. 275 °F,
Time 168 hour
retention after; ASTM D638
Elongation at Break >= 500 %>= 500 %200 mm/min; ASTM D638
 >= 450 %
@Treatment Temp. 135 °C,
Time 605000 sec
>= 450 %
@Treatment Temp. 275 °F,
Time 168 hour
retention after; ASTM D638
Tensile Set <= 175 %
@Treatment Temp. 200 °C,
Pressure 0.200 MPa
<= 175 %
@Treatment Temp. 392 °F,
Pressure 29.0 psi
Elongation, Hot Set Test; IEC 60811-2-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmDC; ASTM D257
Dielectric Constant 2.25
@Frequency 1e+6 Hz
2.25
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 22.0 kV/mm>= 559 kV/inASTM D149
Dissipation Factor 0.00060
@Frequency 1e+6 Hz
0.00060
@Frequency 1e+6 Hz
ASTM D150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9893 / 239409

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.