MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Petropol Durepol® A3 G10 NTLA010 BT309 MSP PBT, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Polyester PBT reinforced with 10% fiberglass, excellent mechanical and thermal properties.

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Water Absorption 0.30 %Humidity Absorption; ASTM D570
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0070 - 0.012 cm/cmASTM D955
Ash 7.0 - 13 %ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 90.0 MPaASTM D638
Elongation at Break 4.8 %ASTM D638
Flexural Strength 140 MPaASTM D790
Izod Impact, Notched (ISO) 6.50 kJ/m²ASTM D256
Charpy Impact, Notched 4.50 kJ/m²ASTM D256
Tensile Creep Modulus, 1 hour 4000 MPaISO 899
Tensile Creep Modulus, 1000 hours 2500 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Dissipation Factor 0.0020
@Thickness 1.00 mm,
Frequency 100 Hz
IEC 60093
 0.0020
@Thickness 1.00 mm,
Frequency 50 Hz
IEC 60093
 0.020
@Thickness 1.00 mm,
Frequency 1e+6 Hz
IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 215 °CASTM D648
Vicat Softening Point 215 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 80.0 °C
Drying Temperature 120 °CStuffing Static (Tray)
Dry Time 6.00 hourStuffing Static (Tray)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL004 / 312912

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.