MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay RHODAFAC® PE-510 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: POLYOXYETHYLENE NONYLPHENYL ETHER, BRANCHED, PHOSPHATE

CAS: 68412-53-3, 68412-54-4, 7664-38-2, 7732-18-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAFAC PE-510 can be used to prepare a broad range of commercial emulsion polymers including acrylics, vinyl-acrylics and styrene-acrylics. Such polymers find application in latex paints, adhesives, paper coatings and textiles. Rhodafac PE-510 is typically converted to its salt form (sodium, ammonium, amine) for use in emulsion polymerization. This is usually done in-situ by neutralization of the diluted phosphate ester with the desired base. Films of polymers made with Rhodafac PE-510 exhibit enhanced corrosion resistance and superior heat and light stability, which makes them especially desirable for metal coating applications. The versatility of Rhodafac PE-510 allows it to be used with a wide range of polymerization techniques, including thermal and redox processes. When properly used in conjunction with other anionic and nonionic surfactants, Rhodafac PE-510 allows for the trouble-free commercial production of extremely stable emulsion polymers.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Surface Tension 32 dynes/cm32 dynes/cmat CMC
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 50 - 5550 - 55KOH to First INFL. PT.; RP-0427
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.80 %<= 0.80 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear liquidat 35°C, RP-0064
 Clear to slightly hazy viscous liquidat 25°C, RP-0064
Color<200APHA, RP-0134
CompositionNonionic Content24-36%, RP-0351
Critical Micelle Concentration (%)0.01
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® HA-70 Surfactant
Solvay RHODAFAC® LO/529-E Surfactant
Solvay RHODAFAC® MB Surfactant
Solvay RHODAFAC® ARB/90 Surfactant
Solvay RHODAFAC® H-66 E Surfactant

WRHOD361 / 137592

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.