MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 226U01 is a one-part, controlled flow adhesive with high temperature resistance.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccCured
Viscosity 250000 cP250000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 909024 hrs @ 75°C
Adhesive Bond Strength 26.9 MPa3900 psiLap shear, alum to alum, 1 hr @ 150°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  45.0 µm/m-°C
@Temperature 20.0 °C
25.0 µin/in-°F
@Temperature 68.0 °F
Alpha 1
 160 µm/m-°C
@Temperature 20.0 °C
88.9 µin/in-°F
@Temperature 68.0 °F
Alpha 2
Glass Transition Temp, Tg 135 °C275 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 
Descriptive Properties
Color Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC073 / 71001

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.