MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI 403 12Cr STAINLESS STEEL BARS FOR TURBINE BLADES (SUS 403-B)
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes:

Creep and rupture data provided by NIMS

Key Words: JIS G4303(91) SUS 403-B; UNS S40300
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170
Tensile Strength, Ultimate 590 MPa
Tensile Strength, Yield 390 MPa
Elongation at Break 25 %
Rupture Strength 42.0 - 49.0 MPa
@Temperature 575 °C,
Time 3.60e+8 sec
 42.0 - 82.0 MPa
@Temperature 550 °C,
Time 3.60e+8 sec
 59.0 - 118 MPa
@Temperature 525 °C,
Time 3.60e+8 sec
 82.0 - 160 MPa
@Temperature 500 °C,
Time 3.60e+8 sec
 111 - 205 MPa
@Temperature 475 °C,
Time 3.60e+8 sec
 157 - 252 MPa
@Temperature 450 °C,
Time 3.60e+8 sec
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 11.5 - 13 %
Iron, Fe 84.68 - 88.5 %
Manganese, Mn <= 1.0 %
Nickel, Ni <= 0.60 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
403 Stainless Steel, annealed, bar
403 Stainless Steel, tempered, bar
AISI 422 12Cr-1Mo-1W-0.3V HEAT RESISTING STEEL BARS FOR TURBINE BLADES (SUH 616-B)
Outokumpu 2205 Duplex Stainless Steel
AISI Type 430F Stainless Steel soft tempered wire 6.4 mm diameter

NIMS018 / 77535

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.