Glass fiber-reinforced and flame retardant polybutylene terephthalate compound. VESTODUR® GF30-FR3 black V307168 is a 30% glass fiber reinforced, semicrystalline thermoplastic compounds for injection molding, based on polybutylene terephthalate (PBT). Test bars made of this compound are rated V-0, self-extinguishing and nondripping. This compound is especially suitable for parts which are subjected to high mechanical and thermal loads and must have a very good flame-resistance. The incorporated flame retardant is non-migrating and does not contain polybrominated diphenyl ethers. The additive has no corrosive effects on metal inserts or neighboring metal parts. The compounds are distinguished for moldings in the electrical and electronical industry. Laser marking with high contrasts is possible. The compounds are supplied as cylindrical pellets in polyethylene packaging. Pigmentation may affect values.Property data for dry samples. Information provided by Evonik. |