MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering H70B Epichlorohydrin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Peroxide Cured, Epichlorohydrin Rubber, 65-75 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. ASTM and ISO designation = GECO.

Applications: Excellent resistance to petroleum based oils and fuels. Becoming widely used in military and automotive applications where its low and high temperature operating range is superior to that of nitrile. Good resistance to water, acide, ozone and weathering.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70°IRHD; ASTM D1415
 71°IRHD, +1 change after 70 hours @ 140°C; ASTM D1415
Tensile Strength, Yield 10.3 MPaASTM D412
 10.918 MPa6% change after 70 hours @ 140°C; ASTM D412
Elongation at Break 281.6 %-12% change after 70 hours @ 140°C; ASTM D412
 320 %ASTM D412
Compression Set 20 %
@Temperature 100 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °CNon-brittle after 3 minutes
 -50.0 °C
Flash Point >= 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epichlorohydrin Rubber (CO, ECO)
Rubatex R475 Epichlorohydrin Rubber Foam Sheet
Trelleborg P650 Epichlorohydrin
Precision Polymer Engineering N75L Nitrile Rubber
Precision Polymer Engineering N70L Nitrile Rubber

PPRECI041 / 57765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.