MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Entec Enflex® EA3555A Styrenic Block, TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Product Description: CCMED TPE 50A NAT is and easy processing elastomer formulated for injection molding applications. This material is non-hydroscopic, has fast setup time, and has excellent mechanical properties. Regulatory Status: CCMED TPE 50A NAT is formulated with medical grade resins and is suspected to be suitable for use in disposable devices classified by the FDA as Class I & Class II.

Availability: North America

Features: Good Processability

Uses: Medical/Healthcare Applications

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  55
@Time 10.0 sec
55
@Time 0.00278 hour
Extruded; ASTM D2240
 58
@Time 10.0 sec
58
@Time 0.00278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 4.81 MPa698 psiASTM D412
Tensile Stress 1.48 MPa
@Strain 100 %
215 psi
@Strain 100 %
ASTM D412
Elongation at Break 570 %570 %ASTM D412
Tear Strength 26.3 kN/m150 pliASTM D624
Compression Set  20 %
@Temperature 22.8 °C,
Time 79200 sec
20 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
 45 %
@Temperature 70.0 °C,
Time 79200 sec
45 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -55.0 °C<= -67.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 179 °C320 - 355 °FHopper, Extrusion
Rear Barrel Temperature 171 - 199 °C340 - 390 °F
Middle Barrel Temperature 229 - 241 °C445 - 465 °F
Front Barrel Temperature 241 - 249 °C465 - 480 °F
Nozzle Temperature 221 - 241 °C430 - 465 °F
Zone 1 229 - 241 °C445 - 465 °F
Zone 3 241 - 249 °C465 - 480 °F
Zone 5 241 - 249 °C465 - 480 °F
Adapter Temperature 229 - 249 °C445 - 480 °F
Die Temperature 229 - 249 °C445 - 480 °F
Melt Temperature 229 - 249 °C445 - 480 °FInjection
 229 - 249 °C445 - 480 °FExtrusion
Mold Temperature 10.0 - 48.9 °C50.0 - 120 °FInjection
Drying Temperature 60.0 - 70.0 °C140 - 158 °FInjection
 60.0 - 70.0 °C140 - 158 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection
 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 50 - 200 rpm50 - 200 rpmInjection
 100 - 200 rpm100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature194°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB582 / 311275

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.