MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® MT12U01 POM, Medical Technology
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Hostaform« MT12U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12U01 is a moderately high flow grade for faster cycling and thin walled injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption at Saturation 0.65 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 65.0 MPa50mm/min; ISO 527-2/1A
Elongation at Break 25 %
Elongation at Yield 9.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2900 MPa50mm/min; ISO 527-2/1A
Flexural Modulus 2800 MPaISO 178
Charpy Impact Unnotched 150 kJ/m²ISO 179/1eU
 140 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2500 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1300 MPaISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-2
Melting Point 166 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 106 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
 190 - 210 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 190 - 200 °C
Zone 4 190 - 210 °C
Die Temperature 190 - 210 °C
Melt Temperature 190 - 210 °C
Drying Temperature 120 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.15 %
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 4.00 MPa
 
Descriptive Properties
Injection moldingYes
Injection speedslow-medium
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Envalior Arnite® T06 202 PBT (European and Asian Grade)
Celanese Hostaform® MT12U03 POM, Medical Technology
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance
Celanese Hostaform® MT12R01 POM, Medical Technology

PHCQ401 / 178856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.