MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with high extrudability.

Performance Features:

  • High microbial resistance
  • Excellent hydrolysis resistance
  • High stability of melt
  • Easy coloring
  • Low temperature flexibility

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccInjection molded parts
Linear Mold Shrinkage 0.0090 in/inInjection molded; ASTM D955
Melt Index of Compound 55 g/10 min
@Load 21.6 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92Injection molded parts; ASTM D2240
Hardness, Shore D 39Injection molded parts; ASTM D2240
Tensile Strength at Break 45.0 MPaInjection molded parts; DIN 53504
Elongation at Break 600 %Injection molded parts; DIN 53504
100% Modulus 0.00910 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.0159 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 660 pliInjection molded parts; ASTM D624
Abrasion 30mm3, Injection molded; DIN 53516
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 35.0 °CInjection
 25.0 - 40.0 °CExtrusion
Middle Barrel Temperature 365 - 383 °FExtrusion
Nozzle Temperature 365 - 392 °FInjection
 374 - 392 °FExtrusion
Adapter Temperature 190 - 200 °CExtrusion
Die Temperature 190 - 200 °CExtrusion
Mold Temperature 68.0 - 122 °FInjection
 
Descriptive Properties
Heating Zone185-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Huntsman IROGRAN® PS 370-202 TPU-Polyester

PHUQ099 / 159472

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.