MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ConocoPhillips Hydroclear® 150 Industrial Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommended for use in a variety of applications which require a pure fluid. Hydroclear Industrial Oil is ideally suited for use as a seal oil, process oil, concrete form oil, deepwell pump drip oil, diluent, extender oil or other similar application. Hydroclear Industrial Oil provides good thermal stability, low volatility and high purity. Hydroclear Industrial Oil is available in seven different viscosity grades to meet the needs of most applications and operating conditions.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.858 g/cc0.0310 lb/in³
Viscosity Measurement 110110Viscosity Index
Saybolt Viscosity at 100°F 167 SUS167 SUS
Saybolt Viscosity at 210°F 45 SUS45 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt32 cSt
Kinematic Viscosity at 100°C (212°F) 5.5 cSt5.5 cSt
ASTM Color 0.500.50
 
Thermal PropertiesMetricEnglishComments
Distillation Temperature 327 °C621 °FDistillation D-2887 IBP
 375 °C707 °FDistillation D-2887 10%
 426 °C799 °FDistillation D-2887 50%
 489 °C912 °FDistillation D-2887 90%
Pour Point -15.0 °C5.00 °F
Flash Point 204 °C400 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45441.4544
 
Descriptive Properties
Aniline Point235°F
Carbon Residue0.06%
Characterization D-20070.1% PolarTest inaccurate with HC base oils
 5.8% Aromatics (fully saturated)Test inaccurate with HC base oils
 94.1% SaturatedTest inaccurate with HC base oils
Composition, Supercritical Fluid Chromatography 0% Aromatics
 0% Polars
 100% Saturates
HPLC Aromatic Detection 1-Ring170 ppm
HPLC Aromatic Detection 2.5-RingNot Detectable
HPLC Aromatic Detection 2-RingMax 1 ppm
HPLC Aromatic Detection 3-Ring and AboveNot Detectable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON094 / 75131

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.