MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA1820 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Petrothene GA1820 resin is a pelletized linear low density polyethylene selected by customers for applications that require maximum strength and toughness. This product offers excellent additive homogeneity, requires no transfer equipment modification, and facilitates clean and safe handling. Typical applications include cast stretch film, blown stretch film, and high end film applications. The GA1820 resin offers enhanced film strength, unitization holding force, drawdown, toughness, and heat seal strength.

Availability: Asia-Pacific; Europe; North America; South & Central America

Application: Blown Stretch Film; Cast Stretch Film; General Purpose Film Packaging; High End Film Applications

Market: Flexible Packaging; Rigid Packaging

Processing Method: Blown Film; Cast Film; Sheet and Profile Extrusion

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
Melt Flow 2.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 380 %Cast Film; ASTM D882
 750 %Blown Film; ASTM D882
Film Elongation at Break, TD 720 %Cast Film; ASTM D882
 900 %Blown Film; ASTM D882
Secant Modulus, MD 0.156 GPa1%, Cast Film; ASTM D882
 0.240 GPa1%, Blown Film; ASTM D882
Secant Modulus, TD 0.183 GPa1%, Cast Film; ASTM D882
 0.290 GPa1%, Blown Film; ASTM D882
Elmendorf Tear Strength MD 430 gCast Film; ASTM D1922
 500 gBlown Film; ASTM D1922
Elmendorf Tear Strength TD 670 gBlown Film; ASTM D1922
 840 gCast Film; ASTM D1922
Dart Drop Test 90.0 gF50, Cast Film; ASTM D1709
 130 gF50, Blown Film; ASTM D1709
Film Tensile Strength at Break, MD 35.0 MPaCast Film; ASTM D882
 56.0 MPaBlown Film; ASTM D882
Film Tensile Strength at Break, TD 22.0 MPaCast Film; ASTM D882
 45.0 MPaBlown Film; ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 2.00 %Cast Film; ASTM D1003
 15.0 %Blown Film; ASTM D1003
Gloss 40.0 %45°, Blown Film; ASTM D2457
 53.0 %45°, Cast Film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9712 / 324647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.