MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 10B Enriched Boron Carbide
Categories: Ceramic

Material Notes: Ceradyne, Inc., a 3M company, offers a range ofenriched boron-10 materials designed for the nuclear power industry. These materials can be isotopically tailored to meet individual customer specifications. 3M™ 10B Enriched Boron Carbide offers excellent thermal stability and gamma discrimination, along with a high thermal neutron absorption cross-section. These properties make 3M 10B enriched boron carbide ideal for applications in neutron detecting technologies. 3M 10B enriched boron carbide can be manufactured to meet existing industry standards, such as ASTM C750 and ASTM C751, or more stringent requirements as required by specific customer applications. Where necessary, naturally occurring isotopic materials can be synthesized to comply with unique purity and stoichiometry requirements. Ceradyne has refined the manufacturing process for enriched boron carbide by using enriched boric acid as a precursor material. This process allows greater flexibility in chemistry and physical properties. For example, we can produce boron carbide with specific B to C ratios, enrichments and particle sizes to meet your specifications.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Boron, B 74 - 77 %74 - 77 %
Carbon, C 23 - 26 %23 - 26 %
Iron, Fe <= 0.10 %<= 0.10 %
 <= 0.10 %<= 0.10 %
 
Descriptive Properties
Impurities<100 ppmManganese
 <100 ppmSodium
 <100 ppmChlorine+Fluorine
 <50 ppmCalcium
 <500 ppmTitanium
 <500 ppmAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Boron Carbide, B4C
American Elements Boron Carbide Nanoparticles
Goodfellow Hot Pressed Boron Carbide B4C
Ceradyne Ceralloy® 546-3E Boron Carbide
Ceradyne Ceralloy® 546 Boron Carbide

PMM40033 / 194924

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.