MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS N07713; AMS 5377; AMS 5391 (Investment Casting)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.91 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 760 MPa
Tensile Strength, Yield >= 690 MPa
Elongation at Break >= 3.0 %
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.5 %
Carbon, C <= 0.20 %
Cb + Ta 1.0 - 3.0 %
Chromium, Cr 13 - 15 %
Molybdenum, Mo 2.5 - 5.5 %
Nickel, Ni 68.55 - 77.05 %As Balance
Titanium, Ti 0.75 - 1.25 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alloy 713C Cast Nickel Superalloy (UNS N07713)
MetalTek IN® 718 UNS N07718 Centri-Vac Nickel Cobalt Based Alloy
Alloy 713LC Cast Nickel Superalloy
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy

NMETEK151 / 18401

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.