MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be present. It is highly resistant to a wide range of inorganic as well as organic acids and hydrocarbon based chemical compounds. The product utilizes a unique reinforcement design allowing it to be highly resistant to thermal cycling exposures up to 180°C (355°F) while maintaining its adhesion and resisting cracking, delamination and permeation. ARC S7 is able to be spray applied via conventional airless spray systems at a wet film thickness of 0.25-0.5 mm (10-20 mils) per coat. ARC S7 may also be applied by brush and roller, though with reduced film build. It is recommended to be applied in two coats for elimination of holidays and pinholes.

Benefits:

  • Resistant to thermal cycling
  • Resistant to cold wall induced blistering
  • ARC S7 is well suited for aggressive chemical exposures at elevated exposures and is easily sprayed with conventional spray equipment
  • ARC S7 does not require a primer and is capable of in-situ curing

Suggested Uses:

  • Flue gas ducts
  • Quench zones
  • Process tanks
  • Storage tanks
  • Steel structures
  • Bag filters
  • Reactor domes

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/ccCured
Volatile Organic Compounds (VOC) Content 550 g/l
@Temperature 43.0 °C
EPA 24
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89ASTM D2240
Elongation at Break 1.04 %ASTM D638
Flexural Strength 7500 psiASTM D790
Flexural Modulus 903000 psiASTM D790
Compressive Strength 16000 psiASTM D695
Adhesive Bond Strength >= 2370 psiASTM D4541
Impact Test 80.0 in-lbdirect; ASTM D2794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °CWet Service (water)
 180 °CDry Service (continuous)
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 29.0 °C
Overcoat Begin
 2.00 hour
@Temperature 21.0 °C
Overcoat Begin
 3.00 hour
@Temperature 29.0 °C
Overcoat End
 4.00 hour
@Temperature 21.0 °C
Overcoat End
 4.50 hour
@Temperature 16.0 °C
Overcoat End
 5.00 hour
@Temperature 10.0 °C
Overcoat End
 6.00 hour
@Temperature 16.0 °C
Overcoat Begin
 12.0 hour
@Temperature 10.0 °C
Overcoat Begin
 16.0 hour
@Temperature 29.0 °C
Full Chemical
 24.0 hour
@Temperature 21.0 °C
Full Chemical
 48.0 hour
@Temperature 16.0 °C
Full Chemical
 72.0 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 1.167 hour
@Temperature 29.0 °C
without MEK
 1.267 hour
@Temperature 29.0 °C
with MEK
 1.67 hour
@Temperature 21.0 °C
without MEK
 2.00 hour
@Temperature 16.0 °C
without MEK
 2.00 hour
@Temperature 21.0 °C
with MEK
 2.33 hour
@Temperature 10.0 °C
without MEK
 3.00 hour
@Temperature 10.0 °C
with MEK
 25.0 hour
@Temperature 16.0 °C
with MEK

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EDRO #7 Shock Resistant S7 Tool Steel
Crucible Steel S7 XL (Premium AISI S7) Tool Steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Crucible Steel S7 (AISI S7) Tool Steel
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)

PPTCHS038 / 138150

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.