MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcal™ ElectroCut™ 7125-114 Graphic Film
Categories: Polymer; Film

Material Notes: 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film colors have a white paper liner; Superior cutting as small as 0.375 in (0.95 cm) and weeding; Ideal for prespaced and electronically cut, screen printed or used in narrow width thermal transfer printing systems

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 63.5 - 88.9 microns2.50 - 3.50 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2490 psi
Peel Strength 0.526 kN/m3.00 pliAdhesion to Polypropylene
 0.701 kN/m4.00 pliAdhesion to ABS
 0.701 kN/m4.00 pliAdhesion to Acrylic
 0.701 kN/m4.00 pliAdhesion to Acrylic enamel
 0.701 kN/m4.00 pliAdhesion to Fruehauf pre-painted panels
 0.701 kN/m4.00 pliAdhesion to Polycarbonate
 0.701 kN/m4.00 pliAdhesion to Urethane paints
 0.877 kN/m5.00 pliAdhesion to Chrome
 1.40 kN/m8.00 pliAdhesion to Aluminum, alodine
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 10.0 °C>= 50.0 °FApplication Temperature, Air and Substrate
 
Descriptive Properties
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34883 / 169630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.