Good stiffness, Moderate toughness, Easy processability Applications: Industrial packaging, Liners, Blends with LLDPE, Foam articles Additives: Base resin Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions. Information provided by NOVA Chemicals. |