MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox 63a Methyl ethyl ketone peroxide and acetylacetone peroxide, in solvent mixture
Categories: Other Engineering Material

Material Notes: Trigonox 63a is a phthalate-free blended initiator for longer working time and faster curing of promoted unsaturated polyester resins at ambient conditions. Used in place of MEKP to extend open time and reduce gel to peak.

CAS number: 1338-23-4, 37187-22-7

EINECS/ELINCS No: 215-661-2; 253-384-9

Applications: Trigonox 63a is phthalate-free blended initiator used for the curing of unsaturated polyester, vinyl ester and acrylic thermoset resins at ambient conditions in conjunction with metal salts. Trigonox 63a provides for a similar gel to MEKP’s with a shorter gel-to-peak interval, resulting in faster demolding in applications such as cast polymer, laminates and RTM. Additional end-use information is available in Nouryon’s application brochures.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 55.0 °C131 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Content6.4-6.6 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1137 / 286660

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.