Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: 30% Glass Fiber Reinforced Additive: Heat Stabilizer Features: Flame Retardant; Heat Stabilized Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |