MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
RESPOL EBANTIX® E1704 EBA
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: EBA REPSOL EBANTIX® E1704 is a copolymer suitable for blown film applications where good processability, flexibility and good mechanical properties are required. The butyl acrylate content is 17%. It contains antioxidant additives.
Applications: Film extrusion; Stretch hood film; Cables
Recommended melt temperature 180°C. Processing characteristics of E1704 are similar to LDPE and conventional polyethylene extruders are recommended. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer, Food Contact Acceptable; Good Flexibility; Good Processability

Uses: Blow Molding Applications; Film

Agency Ratings: EU Food Contact

Processing Method: Blown Film; Film Extrusion

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccISO 1183
Butyl Acrylate Content 17 %
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 750 %
@Thickness 0.102 mm
Blown Film; ISO 527-3
Film Elongation at Break, TD 850 %
@Thickness 0.102 mm
Blown Film; ISO 527-3
Elmendorf Tear Strength MD 367 g
@Thickness 0.102 mm
Blown Film; ISO 6383-2
Elmendorf Tear Strength TD 399 g
@Thickness 0.102 mm
Blown Film; ISO 6383-2
Dart Drop Test >= 1400 g
@Thickness 0.102 mm
Blown Film; ISO 7765-1
Film Tensile Strength at Break, MD 4210 psi
@Thickness 0.102 mm
Blown Film; ISO 527-3
Film Tensile Strength at Break, TD 4350 psi
@Thickness 0.102 mm
Blown Film; ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 205 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESPOL1307 / 312000

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.