MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Tabriz GPPS 1240 Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: GPPS1240 is a crystal polystyrene for extrusion, impact dilution and injection molding application with good mechanical properties. Applications: special extrusion, impact dilution and special injection molding.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 4.30 GPa624 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 96.0 °C205 °F50°C/hr 1kg; ASTM D1525
 
Descriptive Properties
Styrene Residual Monomer<500 ppmCLG LABPSG004 (Atofina Test)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1540(EU) Crystal Polystyrene
Overview of materials for Polystyrene, Transparent Grade
Ineos Nova 3900 General Purpose Crystal Polystyrene
Ineos Nova 3504 General Purpose Crystal Polystyrene
Ineos Nova 2590 General Purpose Crystal Polystyrene

PTABRZ935 / 198241

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.