MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Lucite® 41 Acrylic Resin for Casting and Embedments
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Lucite® 41 is a high molecular weight methyl methacrylate homopolymer for use in castings & embedments.
Like all Lucite® Acrylic Resins for castings & embedments, Lucite® 41 offers: Exceptional Gloss; Very High Surface Hardness and Abrasion Resistance; Sparkle; Crystal Clarity; Outstanding Ultraviolet Light Resistance; Excellent Resistance to Water, Alcohol, Dilute Acids and Alkalis, Chemical Fumes, and Corrosive and Oxidizing Environments
Lucite International’s Lucite® resins production process results in pure product to enable castings and embedments to be manufactured with exceptional optical clarity and sparkle.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0431 lb/in³
Water Absorption 0.47 %0.47 %
Particle Size 75 - 105 µm75 - 105 µm
Viscosity Measurement 1.137 - 1.3671.137 - 1.367Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8181
Tensile Strength 55.0 MPa7980 psi
Elongation at Break 1.0 %1.0 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4911.491
Transmission, Visible 92 %92 %
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.75 %0.75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Abatron Acrylic 57-1™ Clear, Water-Based Coating
INEOS Styrolution Zylar® 960 MBS
Lucite International Lucite® 6751 Acrylic Bead Resin

PLUCIT9493 / 150207

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.