MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Daikin DAI-EL® G-EXP-018 Fluoroelastomer Copolymer, 65% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-EXP-018 is a cure incorporated copolymer with medium Mooney viscosity and moderate cure speed. It is designed for calendering and compression molding, especially for demolding of seals and other complex shapes without tearing.

Typical Applications: O-rings, seals, gaskets, simple molded parts

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/cc
Mooney Viscosity 50
@Temperature 121 °C
50
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373
Tensile Strength at Break 15.6 MPa2260 psi
Elongation at Break 260 %260 %
100% Modulus 4.20 MPa
@Strain 100 %
609 psi
@Strain 100 %
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -18.0 °C-0.400 °FLow Temperature Retraction; ASTM D1329
 
Processing PropertiesMetricEnglishComments
Cure Time 1.20 min0.0200 hourts2, scorch time
 1.50 min0.0250 hourt'50, time to 50% cure
 2.30 min0.0383 hourt'90, time to 90% cure
 10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
Press Cure
 1440 min
@Temperature 232 °C
24.0 hour
@Temperature 450 °F
Post Cure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 65 %65 %
 
Descriptive Properties
ColorWhite to cream
MH16.5 dNmmaximum torque
ML2.1 dNmminimum torque
Test Formula100 phrDAI-EL® G-EXP-018
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9807 / 209878

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.