MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Pyromet 538 Stainless Steel Plate
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Longitudinal orientation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 675 MPa
@Temperature 24.0 °C
 1370 MPa
@Temperature -196 °C
 1490 MPa
@Temperature -269 °C
Tensile Strength, Yield 340 MPa
@Temperature 24.0 °C
 800 MPa
@Temperature -196 °C
 1010 MPa
@Temperature -269 °C
Elongation at Break 52 %
@Temperature -269 °C
 75 %
@Temperature 24.0 °C
 76 %
@Temperature -196 °C
Reduction of Area 59 %
@Temperature -269 °C
 73 %
@Temperature -196 °C
 81 %
@Temperature 24.0 °C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S24000 Stainless Steel, plate
AISI 8742 Alloy Steel Plate, Composition Spec
AIM 70 Fusible Alloy
Phosphorized Admiralty Copper, UNS C44500, OSO60 (0.08mm) Temper strip
Phosphor bronze 10% Sn, UNS C52400, OSO35 Temper wire

MQZ9934 / 172184

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.