MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Yuyao Zhonga PA FRML Nylon6 flame retardant masterbatch
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Flame-retardant masterbatch of PA6 or PA66: keeping its good mechanical properties, ageing resistance, thermal stability and good processability, etc. after adding the master and the flame retardant grade could be changed from UL-94,V0,V1,V2 to HB. The mixture of flame-retardant masterbatch and PA6 can replace flame-retardant PA6 to decrease production cost, so does PA66 and can be used for household electric appliance parts, low voltage electrical apparatus, air switch, electric plug-in unit, communications equipments, lighting luminaire, luminaire, mining electric apparatus parts, etc.

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.60 mm
Proportion: 10%
 V-2
@Thickness 1.60 mm
Proportion: 15%
 V-1
@Thickness 1.60 mm
Proportion: 20%
 V-0
@Thickness 1.60 mm
Proportion: 25%
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 245 °CInjection Temp
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 90.0 - 100 °C
Dry Time 2.00 - 3.00 hour
Injection Pressure 60.0 - 90.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PYUYZ075 / 281868

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.