MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.

Applications: Pearlcoat® D125KW is used to melt coatings on textile substrates for conveyor belts, obtained by sintering (in this case the product is previously ground, so as to be in powder form).

For optimum results, previous drying of the product for 2 hours at 90 - 100°C is advisable, in a hot air circulatory, vacuum or desiccant-air dryer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccDIN 53.479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85DIN 53.505
Tensile Strength 25.0 MPaDIN 53.504
Tensile Stress at Strain 7.50 MPa
@Strain 100 %
DIN 53.504
 11.0 MPa
@Strain 300 %
DIN 53.504
Elongation at Break 520 %DIN 53.504
Abrasion 40mm3 Loss; DIN 53.516
Compression Set 40 %
@Temperature 23.0 °C,
Time 252000 sec
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
DIN 53.517
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 150 °CMelt Range for MFI=10; MQSA 111
Glass Transition Temp, Tg -28.0 °C(DSC, 10°C/min); DIN 51.007
 
Descriptive Properties
Colorwhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C 65 A HPM TPUR
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
ExxonMobil Vistalon™ 706 Ethylene Propylene Copolymer Rubber

PMEQU992 / 109229

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.