MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 1 to 1 by weight.

KONA 877 with HARDENER #112 is a versatile epoxy casting system developed for high performance production potting and encapsulating applications where low shrinkage and rapid air evacuation are required. This formulation has a very low surface tension and a flowable viscosity which affords excellent air release. It has been used as a one fill impregnating and encapsulating resin. KONA 877 with HARDENER #112 adheres to rigid plastics and laminates, metals and ceramics, has a low coefficient of thermal expansion and is readily machined and shaped with ordinary shop tools. The fully cured epoxy system is an excellent electrical insulator which provides good resistance to electrolysis, leakage and corrosion, water, weather, gases and chemical compounds including mild acids and alkalis, many corrosive salts and salt solutions, petroleum products, lubricants and other organic and inorganic materials.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccMixed
Viscosity 3000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Tensile Strength at Break 8000 psi
Compressive Strength 14000 psi
Shear Strength 2500 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 450 V/mil
Dissipation Factor 0.010
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 100 °CHeat distortion temperature, load unknown
 120 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 220 °C
 2.00 hour
@Temperature 150 °C
 48.0 hour
@Temperature 25.0 °C
Pot Life 120 min
@Temperature 25.0 °C
150 g mass
 
Descriptive Properties
ColorBlack or white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
Resin Technology Group 451 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group KONA 870FT-FR Fire Retardant Epoxy Casting System
Resin Technology Group KONA 871 Low Cost Epoxy Resin
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive

PRESINT635 / 65519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.