MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ CCS633LV-MC/CCS-K45-514ML Two component rapid set epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: CCS633LV-MC/CCS-K45-514ML is a general purpose 2 component rapid set epoxy for a wide range of applications. This product will bond most substances. However, due to the wide range of applications, conditions under which applications are accomplished, there can be no assurance that this product will always provide 100% results. It is that preliminary testing and evaluation be done on the product before attempting critical and sensitive application on expensive parts. With proper consideration to surface preparation, mixing, application curing, CCS633LVMC/CCS-K45-514ML provides outstanding results whether drilling, tapping, sanding, patching or bonding. Advantages: Easy Mixing Ratio (1:1 by Volume), Flows easily. Smooth paste consistency, Rapid Set. Develops high strength in 10 to 20 minutes, Bonds to most surfaces, Sands, drills and taps.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 10 %by volume
Water Absorption 0.20 - 0.54 %
Viscosity 13000 - 15000 cPad mix; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Tensile Strength 11400 psi7 days; ASTM D638
Elongation at Break 1.0 - 5.0 %
Compressive Strength 10000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 490 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hourfor quick service
 24.0 hourfor optimum properties
Pot Life >= 3.50 min
@Temperature 24.0 °C
Working Life 5.00 - 7.00 min
@Temperature 25.0 °C
Shelf Life 12.0 Monthfrom mfg. date
 
Descriptive Properties
ColorResin: clear. Hardener: light amber. Mixed: clear to light amber
Mix Ratio1:1 by vol.
Tack Free Time10 to 15 minutes, approx. 60 mils thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI920 / 232180

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.