MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Pibiflex® 3884 Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Pibiflex 3884 is a nominal 38 Shore D thermoplastic polyester elastomer.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
Maximum Moisture Content 0.050
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
@Time 15.0 sec
ISO 868
Tensile Strength at Break 4060 psiISO 527-2/50
Elongation at Break >= 500 %ISO 527-2/50
Tensile Modulus 13100 psiISO 527-1
Izod Impact, Notched (ISO) NB
@Temperature -30.0 °C
ISO 180/1A
 NB
@Temperature 22.8 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 401 °FISO 11357-3
 
Processing PropertiesOriginal ValueComments
Drying Temperature 212 - 230 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6298 / 310991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.