MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It is widely used for applications like connectors and components for appliances.

Key characteristics:

  • High stiffness
  • High strength
  • Low moisture absorption
  • Colorable
  • Good thermal performance
  • UL 94 V0 listing at 0.7 mm

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.63 g/ccASTM D792, ISO 1183
Water Absorption 0.20 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 0.30 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmEuronil
Linear Mold Shrinkage, Transverse 0.0050 cm/cmEuronil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 130 MPaISO 527, ASTM D638
Elongation at Break 2.5 %ISO 527, ASTM D638
Flexural Yield Strength 180 MPaISO 178, ASTM D790
 115 MPa
@Temperature 90.0 °C
ISO 178, ASTM D790
Flexural Modulus 10.0 GPaISO 178, ASTM D790
 5.50 GPa
@Temperature 90.0 °C
ISO 178, ASTM D790
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²ISO 179
 2.50 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.800 J/cm²ISO 179
 0.600 J/cm²
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Comparative Tracking Index 125 V
@Thickness 3.20 mm
Sol. B; IEC 112, UL 746A
 250 V
@Thickness 3.20 mm
Sol. A; IEC 112, UL 746A
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 140 °C20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 221 °CISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °CISO 75, ASTM D648
Vicat Softening Point 200 °C49 N; ISO 306, ASTM D1525
 220 °C9.8 N; ISO 306, ASTM D1525
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Oxygen Index 34 %ASTM D2863
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 694-2-12
 960 °C
@Thickness 0.800 mm
IEC 694-2-12
 
Descriptive Properties
Flammability RatingSEFMVSS No. 302, 355x100x1 mm
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Coolpoly® D4302 Thermally Conductive Polybutylene Terephthalate
Celanese Celanex® 3114 7.5% Fiberglass Reinforced Polybutylene Terephthalate

PLBN63 / 50452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.