MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Pro® 2005 XRC Black 20% Filler Content Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Multi-Pro 2005 XRC is specifically designed for injection molded electronic industrial uses. This product shows higher heat distortion and notched izod than typical glass filled polypropylene. This product is suitable for sonic wielding, is UV stabilized, and has better than average moisture resistance compared to typical glass-filled compounds.

Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792-91
Linear Mold Shrinkage 0.0030 cm/cmASTM D955-89
Melt Flow 7.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 46.0 MPaASTM D638-95
Flexural Strength 61.0 MPaASTM D790-92
Flexural Modulus 2.759 GPaMethod 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.610 J/cmASTM D256-93a
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Eurotec® Tecolen® CP10 GR10 NL PPCP, 10% glass fiber reinforced, natural
E-Polymers TEKAFIN® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP
Celanese Celstran® +PP-GF20-05CN05 Black PP, 20% Glass Reinforced

PLA279 / 49676

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.