MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Algoflon® DF 130 F PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® DF 130 F is a white fine coagulated powder and is produced without any intentional use or addition of PFOA. It is designed for paste extrusion and is particularly recommended for manufacture of porous items and fibers. It can also be used for production of pipe liners (large diameters).

Algoflon® DF 130 exhibits high both green strength and stretchability.

Main features of Algoflon® DF 130 F include:
- High green strength
- High and homogenous stretchability

Applications: Aerospace Applications; Automotive Applications; Electrical/Electronic Applications; Fibers; Industrial Applications; Membranes; Tape; Wire & Cable Applications

Features: Chemical Resistant; Good Processing Stability; Good Thermal Stability; Low Friction

Processing
- Algoflon® DF 130 F is processed according to methods conventionally used for paste extrusion. Initially the powder is mixed with a lubricant to produce a paste. This is then compacted into a preform and extruded through a finishing die using a ram extruder. Further processing as calendering, removal of lubricant and stretching can then be carried out to make final products such as tapes, cords and other general porous items.
- The mixing, preforming, extrusion and heating and stretching steps must all be carefully controlled to produce defect free products.

Storage and Handling
- Algoflon® PTFE fine coagulated powders must be stored and handled carefully to avoid excessive shearing and particle fibrillation. Fibrillation is irreversible and damaged particles can appear as defects in manufactured articles. PTFE fine coagulated powders must be handled below 19°C because above this temperature the powders are softer and can be more easily laminated. It is recommended sieving of powders below 19°C before adding lubricant. Strong vibrations and shocks must be avoided as much as possible for prevent lumps formation. Storage and transportation should be carried out in the range 5 - 19°C. Moreover, the powders must be stored in a dry room because the absorption of moisture could negatively affect its processing. Storage and handling facilities should be clean since even very small foreign particles can cause defects in finished products. Keep resin drums closed and clean. Good housekeeping and careful handling are essential.

- Storage and transportation should be carried out in the range 5 - 19°C. Moreover, the powders must be stored in a dry room because the absorption of moisture could negatively affect its processing.
- Storage and handling facilities should be clean since even very small foreign particles can cause defects in finished products. Keep resin drums closed and clean. Good housekeeping and careful handling are essential.

Safety and Toxicology
- Before using Algoflon® PTFE fine coagulated powders consult the product Material Safety Data Sheet and follow all label directions and handling precautions. As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contacts wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.16 g/ccASTM D792
Bulk Density 0.500 g/ccASTM D4894
Particle Size 600 µmAverage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30.0 MPaASTM D4894
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorWhite
FormsPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4020 / 279820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.