MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Applications:
  • injection molding
  • housing of electrical appliances such as electric fans, telephones, calculators and toys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D785
Tensile Strength, Ultimate 530 kg(f)/cm²
@Temperature 23.0 °C
ASTM D638
Flexural Yield Strength 720 kg(f)/cm²
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 24000 kg(f)/cm²
@Temperature 23.0 °C
ASTM D790
Izod Impact, Notched 27.0 kg-cm/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
@Thickness 6.35 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.35 mm
ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 240 °C
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 18000 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
TPI Porene® ABS-GA800 High Impact ABS Resin
BASF Ultramid® B3S Q661 PA6 (Dry)

PIRPC007 / 83984

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.