MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate.
Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always be purged with LDPE or suitable cleaning compound before shutdown.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
  • Free Flowing Agent: No
Applications:
  • Agricultural Film
  • Blown Film
  • Cast Film
  • Co-Extrusion Films
  • Extrusion Coating
  • Lamination Film
  • Tube Extrusion

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccExxonMobil method
Vinyl Acetate Content 18 %ExxonMobil method
Melt Flow 1.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Elmendorf Tear Strength MD 80 gASTM D1922
Elmendorf Tear Strength TD 180 gASTM D1922
Dart Drop Test 690 gASTM D1709A
Film Tensile Strength at Break, MD 5700 psiASTM D882
Film Tensile Strength at Break, TD 4900 psiASTM D882
1% Secant Modulus, MD 7300 psiASTM D882
1% Secant Modulus, TD 7300 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 187 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 144 °FASTM D1525
 
Descriptive Properties
Blending Temperature240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Escorene™ FL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade)
Arkema OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer
Arkema EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate
Dow Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate

PEX99089 / 175325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.