MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

CRP Technology Windform® FX Black Polyamide for SLS
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Windform® FX Black’s mechanical characteristics make it particularly suited for Additive Manufacturing applications. It guarantees consistent performance on repeatable jobs. It is characterized by exceptional resistance to repeated bending and torsion. The material shows excellent impact resistance even at low temperatures. Its consistency and behavior are similar to polypropylene and ABS injection moulded parts. Windform® FX BLACK is perfect for creating accurate, reliable, and long lasting prototypes. No post-production treatments are needed, as the material has an excellent surface finish in its sintered state. Any additional manual finishing improves its polish. It can be considered a highly valuable material in various functional applications..

Applications IncludeFlexible components and functional parts with living hinges or clip fittings. It is also suitable for ducting of complex shapes, or for thin walled connectors with snap-fit systems. Improvements in detail reproduction make Windform® FX BLACK suitable for applications which require accurate and superior definition. Windform® FX BLACK is the material of choice for flexible components with fine details.

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.022 g/cc0.03692 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.74 MPa7359 psiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 50.3 %50.3 %UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 1.908 GPa276.7 ksiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 67.60 MPa9805 psiUNI EN ISO 14125: 2000
Flexural Modulus 1.820 GPa264.0 ksiUNI EN ISO 14125: 2000
Charpy Impact Unnotched  21.76 J/cm²
@Temperature -40.0 °C
103.6 ft-lb/in²
@Temperature -40.0 °F
Completely broken specimens; UNI EN ISO 179-1
 25.44 J/cm²
@Temperature 23.0 °C
121.1 ft-lb/in²
@Temperature 73.4 °F
Completely broken specimens; UNI EN ISO 179-1
Charpy Impact, Notched  0.422 J/cm²
@Temperature -40.0 °C
2.01 ft-lb/in²
@Temperature -40.0 °F
UNI EN ISO 179-1
 2.169 J/cm²
@Temperature 23.0 °C
10.32 ft-lb/in²
@Temperature 73.4 °F
UNI EN ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.7e+15 ohm-cm3.7e+15 ohm-cmASTM D257-93
Surface Resistance 9.7e+15 ohm9.7e+15 ohmASTM D257-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 198.7 °C389.7 °FISO 11357-2
Deflection Temperature at 1.8 MPa (264 psi) 52.1 °C126 °FASTM D 648 TYPE B
Vicat Softening Point 190.5 °C374.9 °F10 N; ASTM D1525-09
 
Descriptive Properties
ColorBlack
Specific Flexural Modulus1781[MPa/(g/cc)], Flexural Modulus per density unit
Specific Flexural Strength66.1[MPa/(g/cc)], Flexural Strength per density unit
Specific Tensile Modulus1867[MPa/(g/cc)], Tensile Modulus per density unit
Specific Tensile Strength49.7[MPa/(g/cc)], UTS per density unit
Surface Finish0.80 Ra µmAfter CNC machining
 1.60 Ra µmAfter Manual Finishing
 5.00 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ALM FR 106 Nylon 11 SLS Prototyping Polymer
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
ALM PA 615-GF Nylon 12 SLS Prototyping Polymer, 50% Glass Filled
ALM PA 250 Nylon 12 SLS Prototyping Polymer

PCRPT00a9 / 209870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.