MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-481 PAEK
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Unreinforced

Material Notes: AvaSpire® AV-481 is an unreinforced PAEK (polyaryletherketone) that offers improved ductility and impact strength relative to PEEK while offering similar or superior melt processability to high melt flow PEEK that is available on the market. Chemical resistance and environmental stress cracking resistance of AV-481 are also on par with that of unreinforced PEEK. This product has been specifically formulated for applications requiring an excellent balance of chemical resistance and mechanical toughness along with very high melt flow characteristics to allow filling of very thin and long flow length parts like cable ties. The heat resistance of this grade is also quite high with a heat distortion temperature in excess of 200°C and very good long term oxidative stability at elevated temperatures. This combination of properties makes AV-481 well-suited for applications in automotive, aerospace, electrical/electronics, and other industrial uses.
AvaSpire® AV-481 is an injection molding grade and can be easily processed by typical injection molding methods using standard equipment. The material is available in beige (AV-481 BG15). Because the material is naturally lighter in color than typical PEEK resin, AV-481 provides greater versatility in its ability to be colored.

- Beige: AV-481 BG 15

Applications: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications

Features: Chemical Resistant; Ductile; Fatigue Resistant; Good Dimensional Stability; Good Impact Resistance; High Flow; High Heat Resistance

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Viscosity 170 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
170 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Melt Flow 55 g/10 min
@Load 2.16 kg,
Temperature 400 °C
55 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 97.0 MPa14100 psiASTM D638
Elongation at Break >= 15 %>= 15 %ASTM D638
Elongation at Yield 6.3 %6.3 %ASTM D638
Tensile Modulus 3.20 GPa464 ksiASTM D638
Flexural Strength 141 MPa20500 psiASTM D790
Flexural Modulus 3.30 GPa479 ksiASTM D790
Izod Impact, Notched 0.640 J/cm1.20 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
Dart Drop, Total Energy 78.0 J57.5 ft-lbInstrumented Dart Impact; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
@Thickness 3.20 mm
406 °F
@Thickness 0.126 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 355 °C671 °F
Middle Barrel Temperature 365 °C689 °F
Front Barrel Temperature 370 °C698 °F
Nozzle Temperature 375 °C707 °F
Mold Temperature 175 - 205 °C347 - 401 °F
Drying Temperature 150 °C
@Time 14400 sec
302 °F
@Time 4.00 hour
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBeige
FormsPellets
Injection RateFast
ProcessingInjection Molding
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4145 / 279945

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.